Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Creep Modulus, 1000 hours | 220 MPa | 31900 psi | ISO 899-1 |
Polymer Industries Polyslick UHMW Rod Polyslick UHMW Rod exhibits all of the durable qualities of our Polyslick UHMW Sheet making it perfect for the application where sheet stock is not suitable. The material is ideally suited for the m.. |
|||
Tensile Creep Modulus, 1000 hours | 220 MPa | 31900 psi | ISO 899-1 |
Polymer Industries Polyslick UHMW Sheet Polyslick UHMW Sheet exhibits the properties of excellent impact strength, abrasion resistance, low coefficient of friction, as well as very good chemical resistance. This industrial grade material .. |
|||
Tensile Creep Modulus, 1000 hours | 220 MPa | 31900 psi | ISO 899-1 |
Polymer Industries Polyslick UHMW Profile Polyslick UHMW Profiles exhibit all of the durable qualities of our Polyslick UHMW Sheet making them perfect for use where sheet stock is not suitable. Polymer Industries offers a large variety of p.. |
|||
Tensile Creep Modulus, 1000 hours | 220 - 440 MPa | 31900 - 63800 psi | Average value: 349 MPa Grade Count:7 |
Overview of materials for Polypropylene, Molded This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene, Molded". Each property range of values reported is minimum and maximum values of appropri.. |
|||
Tensile Creep Modulus, 1000 hours | 220 MPa | 31900 psi | |
BASF Novolen® 2500 H Polypropylene Injection molded parts, blow moldings and thermoformed parts.Data was collected by ISO methods and provided by BASF. |