Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Creep Modulus, 1000 hours | 310 MPa | 45000 psi | |
LyondellBasell Lupolen® 5621 D HDPE Data was collected by ISO methods and originally provided by BASF. The Lupolen® product line is now produced by Basell. |