Mechanical Properties Metric English Comments
Tensile Creep Modulus, 1000 hours 2750 MPa

@Strain <=0.500 %
399000 psi

@Strain <=0.500 %
ISO 899-1
BASF Ultraform® N2720 M63 30% Mineral Filled POM
Description: Is a POM, 30 % mineral-reinforced material for low-warpage moldings with high stiffness, strength and hardness.Information provided by BASF