Polymer Property : Tensile Creep Modulus, 1000 hours = 2700 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Creep Modulus, 1000 hours 1300 - 2700 MPa
189000 - 392000 psi
Average value: 2150 MPa Grade Count:4
Overview of materials for Polybutylene Terephthalate (PBT), Glass Bead Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), Glass Bead Filled". Each property range of values reported is minimum ..