Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tenacity | 0.680 N/tex | 7.70 g/denier | 1.35 lb. load |
Shakespeare WonderThread® SN-38 High tenacity TEX# 8 Nylon Industrial Sewing Thread Used for sewing: Bedspreads, Comforters, Caps, Hats, Blankets, Stuffed Toys, Pillows, Carpets and Rugs, Handbags, Indoor Furniture, Curtains and Drapes, Apparel, Sleeping BagsInformation provided b.. |
|||
Tenacity | 0.680 N/tex | 7.70 g/denier | Knot Strength |
UBE 7034T Nylon 6/12 Monofilament (Drawing Ratio=6.5, Diameter 0.4 mm) Specialties: High viscosity Nylon 6/12 Copolymer, High stretch-ability results higher line strength than 50 series, Lower moisture absorption keeps superior physical property even in the waterApplic.. |