Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tenacity | 0.417 - 0.509 N/tex | 4.72 - 5.77 g/denier | |
EMS-Griltech Grilon® XC 130 Nylon 610 Monofilament (Non-Set) Description: GRILON XC 130 is a Nylon 610 based monofilament for press felt fabric.Special Note: GRILON Monofilament has been bought by ShakespeareData provided by EMS-Griltech. |
|||
Tenacity | 0.417 - 0.509 N/tex | 4.72 - 5.77 g/denier | |
EMS-Griltech Grilon® XC 133 Nylon 610 Monofilament (Medium-Set) Description: GRILON XC 133 is a Nylon 610 based monofilament for press felt fabric.Special Note: GRILON Monofilament has been bought by ShakespeareData provided by EMS-Griltech. |