Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tenacity | 0.347 - 0.446 N/tex | 3.93 - 5.05 g/denier | |
EMS-Griltech Grilamid® DN 10 Nylon 12 Monofilament Description: GRILAMID Monofilaments are mainly used in Filtration. Data provided by Description: GRILAMID Monofilaments are mainly used in Filtration. Data provided by EMS-Griltech. |