Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tenacity | 2.38 N/tex | 27.0 g/denier | Tensile Modulus |
UBE 1022T Nylon 6 Monofilament (Drawing Ratio=4.8) Specialties: Medium viscosity Nylon 6 Homopolymer Applications: Fishing net, Small size monofilament, General applicationInformation provided by UBE. |