Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tenacity | 0.777 N/tex | 8.80 g/denier | Line Strength |
UBE 7034T Nylon 6/12 Monofilament (Drawing Ratio=6, Diameter 0.4 mm) Specialties: High viscosity Nylon 6/12 Copolymer, High stretch-ability results higher line strength than 50 series, Lower moisture absorption keeps superior physical property even in the waterApplic.. |