Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tenacity | 0.724 N/tex | 8.20 g/denier | Line Strength |
UBE 5033T Nylon 6/66 Monofilament (Drawing Ratio=5.5) Specialties: High viscosity Nylon 6/66 Copolymer, High transparent and tenacity, Higher drawing ratio can be achieved for superior line strengthApplications: Small-medium size sport fishing line Inf.. |