Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tenacity | 0.653 N/tex | 7.40 g/denier | Line Strength |
UBE 1022T Nylon 6 Monofilament (Drawing Ratio=4.8) Specialties: Medium viscosity Nylon 6 Homopolymer Applications: Fishing net, Small size monofilament, General applicationInformation provided by UBE. |
|||
Tenacity | 0.653 N/tex | 7.40 g/denier | Knot Strength |
UBE 5033T Nylon 6/66 Monofilament (Drawing Ratio=5.5) Specialties: High viscosity Nylon 6/66 Copolymer, High transparent and tenacity, Higher drawing ratio can be achieved for superior line strengthApplications: Small-medium size sport fishing line Inf.. |
|||
Tenacity | 0.653 N/tex | 7.40 g/denier | Knot Strength |
UBE 7034T Nylon 6/12 Monofilament (Drawing Ratio=5.5, Diameter 0.4 mm) Specialties: High viscosity Nylon 6/12 Copolymer, High stretch-ability results higher line strength than 50 series, Lower moisture absorption keeps superior physical property even in the waterApplic.. |
|||
Tenacity | 0.653 N/tex | 7.40 g/denier | Line Strength |
UBE 1022MT2 Nylon 6 Monofilament (Drawing Ratio=4.8) Specialties: Monomer containing type of 1022TApplications: Fishing net, Small size monofilament, Softness required applicationsInformation provided by UBE. |