Polymer Property : Tenacity = 0.618 N/tex Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tenacity 0.618 N/tex
7.00 g/denier
Knot Strength
UBE 5033T Nylon 6/66 Monofilament (Drawing Ratio=5)
Specialties: High viscosity Nylon 6/66 Copolymer, High transparent and tenacity, Higher drawing ratio can be achieved for superior line strengthApplications: Small-medium size sport fishing line Inf..
Tenacity 0.618 N/tex
7.00 g/denier
Tensile Modulus
UBE 7034MT2 Nylon 6/12 Monofilament (Drawing Ratio=5)
Specialties: Monomer containing type of 7034T, High softness Applications: Small-big size sport fishing line and long line (branch line), Softness required applicationsInformation provided by UBE.
Tenacity 0.618 N/tex
7.00 g/denier
Tensile Modulus
UBE 5034MT2 Nylon 6/66 Monofilament (Drawing Ratio=5)
Specialties: Monomer containing type of 5034T, High softness Applications: Small-big size sport fishing line and long line (main line), Softness required applicationsInformation provided by UBE.
Tenacity 0.618 N/tex
7.00 g/denier
Line Strength
UBE 7034T Nylon 6/12 Monofilament (Drawing Ratio=6, Diameter 2 mm)
Specialties: High viscosity Nylon 6/12 Copolymer, High stretch-ability results higher line strength than 50 series, Lower moisture absorption keeps superior physical property even in the waterApplic..