Tenacity 0.583 N/tex
6.60 g/denier
4.8 lb. load
Shakespeare WonderThread® SN-38 High tenacity TEX# 35 Nylon Industrial Sewing Thread
Used for sewing: Bedspreads, Comforters, Caps, Hats, Blankets, Stuffed Toys, Pillows, Carpets and Rugs, Handbags, Indoor Furniture, Curtains and Drapes, Apparel, Sleeping BagsInformation provided b..
Tenacity 0.583 N/tex
6.60 g/denier
Line Strength
UBE 1022MT2 Nylon 6 Monofilament (Drawing Ratio=4.5)
Specialties: Monomer containing type of 1022TApplications: Fishing net, Small size monofilament, Softness required applicationsInformation provided by UBE.
Tenacity 0.583 N/tex
6.60 g/denier
Line Strength
UBE 1022T Nylon 6 Monofilament (Drawing Ratio=4.5)
Specialties: Medium viscosity Nylon 6 Homopolymer Applications: Fishing net, Small size monofilament, General applicationInformation provided by UBE.