Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tenacity | 0.565 N/tex | 6.40 g/denier | Line Strength |
UBE 5034MTAX1 Nylon 6/66 Monofilament (Drawing Ratio=6) Specialties: Excellent transparency and softness, Specially developed for very big size diameter (over 2mm in diameter)Applications: Big size diameter and high transparency required applications (ov.. |
|||
Tenacity | 0.565 N/tex | 6.40 g/denier | Knot Strength |
UBE 7034T Nylon 6/12 Monofilament (Drawing Ratio=5, Diameter 0.4 mm) Specialties: High viscosity Nylon 6/12 Copolymer, High stretch-ability results higher line strength than 50 series, Lower moisture absorption keeps superior physical property even in the waterApplic.. |