Polymer Property : Tenacity = 0.556 N/tex Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tenacity 0.556 N/tex
6.30 g/denier
Line Strength
UBE 5021T Nylon 6/66 Monofilament (Drawing Ratio=4.5)
Specialties: Medium viscosity Nylon 6/66 Copolymer, High knot strength (for Knot improvement), Softness is similar with 1022MT2 (At the heat setting of the net, higher shrink ratio may be expected t..