Polymer Property : Tenacity = 0.512 N/tex Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tenacity 0.512 N/tex
5.80 g/denier
Shakespeare Resistat® F901 R080 Nylon 66 Monofilament
Resistat F901, MERGE R080 is a 80-denier nylon 6,6 monofilament which has electrically conductive carbon suffused into the surface. The filament has a round cross section with a coating thickness o..