Polymer Property : Tenacity = 0.450 N/tex Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tenacity 0.450 N/tex
5.10 g/denier
1.45 lb. load
Shakespeare WonderThread® SN-40 ultra soft TEX# 14 Nylon Industrial Sewing Thread
Used for sewing: Bedspreads, Comforters, Caps, Hats, Blankets, Stuffed Toys, Pillows, Carpets and Rugs, Handbags, Indoor Furniture, Curtains and Drapes, Apparel, Sleeping BagsInformation provided b..
Tenacity 0.450 N/tex
5.10 g/denier
GB/T14337-2008
Sichuan Deyang Haton® 1.5 dtex Polyphenylene Sulfide Staple Fiber
Excellent chemical stabilityInformation provided by Sichuan Deyang Chemical Co., LTD
Tenacity 0.450 N/tex
5.10 g/denier
Knot Strength
UBE 1022T Nylon 6 Monofilament (Drawing Ratio=4.8)
Specialties: Medium viscosity Nylon 6 Homopolymer Applications: Fishing net, Small size monofilament, General applicationInformation provided by UBE.
Tenacity 0.450 N/tex
5.10 g/denier
Line Strength
UBE 7034MT2 Nylon 6/12 Monofilament (Drawing Ratio=5.5)
Specialties: Monomer containing type of 7034T, High softness Applications: Small-big size sport fishing line and long line (branch line), Softness required applicationsInformation provided by UBE.