Mechanical Properties Metric English Comments
Tenacity 0.430 N/tex
4.87 g/denier
GB/T14337-2008
Sichuan Deyang Haton® 2.2 dtex Polyphenylene Sulfide Staple Fiber
Excellent chemical stabilityInformation provided by Sichuan Deyang Chemical Co., LTD
Tenacity 0.430 N/tex
4.87 g/denier
GB/T14337-2008
Sichuan Deyang Haton® 220 dtex Polyphenylene Sulfide Filament
Excellent chemical stabilityInformation provided by Sichuan Deyang Chemical Co., LTD