Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tenacity | 0.297 - 0.396 N/tex | 3.37 - 4.49 g/denier | |
EMS-Griltech Grilamid® DM 10 Nylon 12 Monofilament Description: GRILAMID Monofilaments are mainly used in Filtration. Data provided by EMS-Griltech. |