Mechanical Properties Metric English Comments
Tenacity 0.335 - 0.371 N/tex
3.80 - 4.20 g/denier
Intercontinental Polymers Deniers 3-10 Polyester Staple Fibers, Deniers 3 - 10
Cut Lengths (Inches): 1, 1.25, 1.75, 2, 3 & 4. Lusters: Bright and Semi-Dull. Cross-Section: Round. Specialties: Optical Black, Spun-Dyed Black, Flame Retardant (US and European Standards), Cati..
Tenacity >= 0.335 N/tex
>= 3.80 g/denier
Shakespeare FGP-102 Polyester Monofilament
For food contact applicationsInformation provided by Shakespeare Company.
Tenacity 0.335 N/tex
3.80 g/denier
Shakespeare Resistat® F9416 M040 Nylon 66 Monofilament
Resistat F9416, MERGE M040 is composed of forty filaments of conductive nylon 6,6 yarn. This yarn is twisted and heatset. Each filament has electrically conductive carbon suffused into the surface..
Tenacity 0.335 N/tex
3.80 g/denier
Knot Strength
UBE 5034T Nylon 6/66 Monofilament (Drawing Ratio=4.5)
Specialties: High viscosity Nylon 6/66 Copolymer, Higher transparent and softness than 5033T, High tenacity Applications: Small size sport fishing line and long- line (main line)Information provided..