Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tenacity | 0.327 N/tex | 3.70 g/denier | |
Shakespeare Resistat® F901 R055 Nylon 6 Monofilament Resistat F901, MERGE R055 is a 55-denier nylon 6 monofilament which has electrically conductive carbon suffused into the surface. The filament has a round cross section with a coating thickness of .. |