Mechanical Properties Metric English Comments
Tenacity 0.212 - 0.282 N/tex
2.40 - 3.20 g/denier
LFL-09
Intercontinental Polymers 1171 Bicomponent HDPE/PET Fiber Type - Denier 1.8 X 1.5 Inches
50/50 HDPE Sheath/PET Core. Luster: Semi-Dull. Finish: Hydrophilic.Applications of bicomponent polyester fiber: Absorbent products, hygiene products, non-wovens, filtration, sliver knit, microdeni..