Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Heat Seal Strength Initiation Temperature | 390 °C | 734 °F | 15 min |
Ferro EG 2020 Low-Temperature Sealing VITREOUS, COMPOSITE Typical Powder Form: VEG Ferro's line of low-temperature sealing glasses are comprised of lead-borate (vitreous) and lead-zinc-borate crystallizing glasses formulated to meet sp.. |