Polymer Property : Heat Seal Strength Initiation Temperature = 600 °C Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Heat Seal Strength Initiation Temperature 600 °C
1110 °F
30 min
Ferro CF 7586 Low-Temperature Sealing
DEVITRIFYING Typical Powder Form: TF Ferro's line of low-temperature sealing glasses are comprised of lead-borate (vitreous) and lead-zinc-borate crystallizing glasses formulated to meet specific t..
Heat Seal Strength Initiation Temperature 600 °C
1110 °F
15 min
Ferro EG 2759 Low-Temperature Sealing
VITREOUS, COMPOSITE Typical Powder Form: VEG Ferro's line of low-temperature sealing glasses are comprised of lead-borate (vitreous) and lead-zinc-borate crystallizing glasses formulated to meet sp..