Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Heat Seal Strength Initiation Temperature | 106.1 °C | 223.0 °F | 1.2 mil |
LyondellBasell Adsylâ„¢ 5 C 30 F Polyolefin Description: Adsylâ„¢ 5 C 30 F is a new thermoplastic polyolefin which has been designed as a BOPP sealing layer material with exceptionally low sealing temperature. It features a high clarity a.. |