Polymer Property : Heat Seal Strength Initiation Temperature = 199 °F Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Heat Seal Strength Initiation Temperature 93.0 °C
199 °F
2 lb/in heat seal strength; 0.5 sec dwell, 40 psi bar pressure, pull speed 10 (in./min.); Dow Method
Dow AFFINITY™ PL 1840G Polyolefin Plastomer (POP)
AFFINITY™ PL 1840G is an ethylene alpha-olefin resin produced via INSITE™ Technologies. It is designed to provide blown film with low temperature sealability, good puncture resistance, optics and..