Polymer Property : Heat Seal Strength Initiation Temperature = 157 °C Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Heat Seal Strength Initiation Temperature 157 °C
315 °F
0.40 lb/in heat seal strength; SWTM-19
Dow SARAN WRAP™ 3 Plastic Film
SARAN WRAP™ 3 Plastic Film is a clear biaxially oriented monolayer barrier film, designed for tight wrap and heat sealing applications. It is available in 50 gauge, as single or double would rolls..