Polymer Property : Heat Seal Strength Initiation Temperature = 124 °C Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Heat Seal Strength Initiation Temperature 124 °C
255 °F
Minimum seal strength is 200 g/in at 15 psi pressure and 1 sec.; ASTM D1709
Total PPR 8650 Polypropylene, Random Copolymer
ATOFINA 8650 is a low melting, high ethylene random copolymer with improved color, optics and impact properties. The low melting point of ATOFINA 8650 makes it an excellent heat seal layer for orie..