Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Secant Modulus, TD | 0.2471 GPa | 35.84 ksi | 2% Secant; ASTM D882 |
Dow DOWLEX™ 2045.11G Linear Low Density Polyethylene For high speed, thin film applications Additional thermal stability Complies with U.S. FDA 21 CFR 177.1520 (c) 3.2a Information provided by Dow |