Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Secant Modulus, TD | 0.225 GPa | 32.6 ksi | ASTM D882 |
ExxonMobil Escorene® LD-102 LDPE Drawdown Resin, 0.5 mil Film
(discontinued **) Data provided by the manufacturer, Exxon Chemical.A homopolymer, good clarity, laundry and dry cleaning film resin capable of providing a tough film in very thin gauges.Applications: Dry cleaning es.. |