Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Secant Modulus, TD | 0.2081 GPa | 30.18 ksi | 2% Secant; ASTM D882 |
Dow 621I Low Density Polyethylene (LDPE) Specialty resin designed for high melt strength applications Provides excellent bubble stability Complies with U.S. FDA 21 CFR 177.1520 (c) 2.1 Information provided by Dow |