Mechanical Properties Metric English Comments
Secant Modulus, TD 1.825 GPa
264.7 ksi
Tangent; ASTM D882
Eastman Cadence™ GS5 Clear (Unpigmented) Copolyester for film calendering
Eastman Cadence™ copolyester, for calendered films, is a specialty plastic developed to meet the demand for an environmentally responsible material for the calendering industry. Available in diffe..