Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Secant Modulus, TD = 23.9 ksi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Secant Modulus, TD 0.165 GPa
23.9 ksi
ASTM D882
Chevron Phillips MarFlex® 5428 LDPE Cast Film Resin
Resin Type: HomopolymerCharacteristics: Excellent OpenabilitySuited for high speed convertingGood clarityLow COFApplications: Bakery FilmBreak BagsInformation provided by Chevron Phillips.
Secant Modulus, TD 0.165 GPa
23.9 ksi
2% Secant; ASTM D882
Dow INTEGRAL™ 936 High Heat Monolayer Adhesive Film
INTEGRAL 936 High Heat Monolayer Adhesive Film is a heat-activated, thermally stable adhesive film for automotive applications capable of bonding to urethane foam-baked fabrics, paper, cardboard, fi..
Copyright © lookpolymers.com All Rights Reserved