Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Secant Modulus, TD | 0.145 GPa | 21.0 ksi | ASTM D882 |
Huntsman PE5080 Extrusion Coating Polyethylene
(discontinued **) Homopolymer and FDA compliant.Features: Excellent draw down, low neck-in, and excellent adhesion.Applications: Extrusion: coating grade and thin coatings.FDA Notes: Conforms to FDA regulation 21 CFR.. |
|||
Secant Modulus, TD | 0.145 GPa | 21.0 ksi | ASTM D882 |
Huntsman PE 1402 EVA Film Extrusion
(discontinued **) 4% Vinyl Acetate EVA copolymer and FDA compliantFeatures: Excellent balance of optical and strength, toughness and flexibility at low temperatures, and good heat seal characteristic.Applications: Fi.. |
|||
Secant Modulus, TD | 0.145 GPa | 21.0 ksi | 2% Secant; ASTM D882 |
Dow INTEGRAL™ 933 Tough Film for Lamination to Porous Substrates INTEGRAL 933 Adhesive Film has a low melting, high flow adhesive layer that is useful for bonding to substrates such as polyurethane or polyethylene foam, or to non-woven textiles.Information provid.. |
|||
Secant Modulus, TD | 0.145 GPa | 21.0 ksi | ASTM D882 |
Huntsman Rexell® L3102 Blown Film Extrusion LLDPE
(discontinued **) Linear-low density copolymer, cast film extrusion, FDA compliant.Features: Good impact and puncture resistance with excellent optics and sealability.Applications: Laminated and coextruded films for .. |
|||
Secant Modulus, TD | 0.145 GPa | 21.0 ksi | ASTM D882 |
Huntsman PE1451 EVA Film Extrusion
(discontinued **) 4.5% Vinyl Acetate EVA copolymer and FDA compliantFeatures: Excellent balance of optical and strength, toughness and flexibility at low temperatures, and good heat seal characteristic.Applications: .. |