Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Secant Modulus, TD | 1.241 - 1.517 GPa | 180.0 - 220.0 ksi | ASTM D882 |
Honeywell ACLAR® Rx 160 CTFE Homopolymer, Barrier Film Description: Aclar® Rx160 is a 0.60 mil (15 micron) PCTFE homopolymer, high performance barrier film for the pharmaceutical and medical markets. It thermoforms well on conventional blister packag.. |
|||
Secant Modulus, TD | 1.241 - 1.517 GPa | 180.0 - 220.0 ksi | ASTM D882 |
Honeywell ACLAR® Rx20E CTFE Homopolymer, Barrier Film Description: ACLAR® Rx20Eis a .8 mil CTFE homopolymer high performance barrier film for the pharmaceutical and medical markets. It thermoforms well on conventional blister packaging equipment.Inf.. |