Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Secant Modulus, TD | 1.034 - 1.103 GPa | 150.0 - 160.0 ksi | ASTM D882 |
Honeywell ACLAR® 22A (2.00 mil) Copolymer Film
(discontinued **) Description: ACLAR® 22A is a copolymer film consisting primarily of chlorotrifluoroethylene (CTFE). It is a flexible transparent film used to package moisture sensitive products.Information provide.. |
|||
Secant Modulus, TD | 1.034 - 1.103 GPa | 150.0 - 160.0 ksi | ASTM D882 |
Honeywell ACLAR® 22A (1.50 mil) Copolymer Film
(discontinued **) Description: ACLAR® 22A is a copolymer film consisting primarily of chlorotrifluoroethylene (CTFE). It is a flexible transparent film used to package moisture sensitive products.Information provide.. |