Polymer Property : Secant Modulus, TD = 140 ksi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Secant Modulus, TD 0.965 GPa
140 ksi
ASTM D882
DuPont™ Dartek® SF-502 Nylon 6,6 Super Formable Film, 76 µm Thickness  (discontinued **)
Data provided by DuPont Packaging Polymers.The SF (Super Formable) films are modified blends of nylon 6,6 which enhance the thermoforming characteristic of the Dartek® F series of films Can be used..