Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Secant Modulus, TD | 0.883 GPa | 128 ksi | at 1%; ASTM D882 |
Chevron Phillips K-Resin® KR10 Styrene-Butadiene Copolymer, Film Grade
(discontinued **) Styrene-Butadiene Copolymer. Properties below based on 1 mil ( 0.025 mm) film; 2.5:1 Blow Up Ratio; 35 mil (0.90 mm) die gap.Customer Benefits: This SBC is easily processed on blown film or cast fi.. |
|||
Secant Modulus, TD | 0.883 GPa | 128 ksi | at 1%; ASTM D882 |
Chevron Phillips K-Resin® DK11 Styrene-Butadiene Copolymer, Film Grade Styrene-Butadiene Copolymer. Properties below based on 1 mil ( 0.025 mm) film; 2.5:1 Blow Up Ratio; 35 mil (0.90 mm) die gap.Customer Benefits: Provides the same high performance film properties as.. |