Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Secant Modulus, TD | 0.0790 GPa | 11.5 ksi | 2% Secant Modulus; ASTM-D882 |
Braskem TN2020 EVA General Film Copolymer TN2020 is an Ethylene-Vinyl Acetate (EVA) copolymer developed to mostly meet the needs of the multi-layer packaging segment produced by coextrusion and/or lamination processes. Multilayer structures.. |