Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Secant Modulus, TD | 1.93 GPa | 280 ksi | ASTM D882 |
DuPont™ Dartek® UF-410 Nylon 6,6 Oriented Film, 15 µm Thickness
(discontinued **) Data provided by DuPont Packaging Polymers.A monoaxially oriented nylon 6,6 film with good "slip" characteristics, which ensure excellent machinability/runnability even at high relative humidity con.. |