Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Secant Modulus, TD | 1.50 GPa | 218 ksi | ASTM D882 |
Honeywell Oxyshieldâ„¢ BOEB Biaxially Oriented, Co-Extruded Nylon 6/EVOH/Nylon 6 Clear Film Description: Oxyshieldâ„¢ BOEB is a 0.60 mil (15 micron) biaxially oriented, coextruded nylon 6/EVOH/nylon 6 clear film having excellent gas barrier through a broad range of relative humidity. T.. |
|||
Secant Modulus, TD | 1.50 GPa | 218 ksi | ASTM D882 |
Solvay Specialty Polymers Ajedium™ Films -- Halar® 500LC Ethylene Chlorotrifluoroethylene Copolymer (ECTFE) Halar® ECTFE is a semi-crystalline fluoropolymer with a chemical structure of a 1:1 alternating copolymer of ethylene and chlorotrifluoroethylene.Halar® film is a strong, hard, tough, abrasion.. |