Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Secant Modulus, TD | 1.31 - 1.517 GPa | 190 - 220.0 ksi | ASTM D882 |
Honeywell ACLAR® 33C (2.00 mil) Copolymer Film
(discontinued **) Description: ACLAR® 33C is a copolymer film consisting primarily of chlorotrifluoroethylene (CTFE). 33C is used for military and industrial packaging applications.Information provided by Honeywell.. |
|||
Secant Modulus, TD | 1.31 - 1.586 GPa | 190 - 230.0 ksi | ASTM D882 |
Honeywell ACLAR® 33C (0.75 mil) Copolymer Film
(discontinued **) Description: ACLAR® 33C is a copolymer film consisting primarily of chlorotrifluoroethylene (CTFE). 33C is used for military and industrial packaging applications.Information provided by Honeywell.. |
|||
Secant Modulus, TD | 1.31 - 1.724 GPa | 190 - 250.0 ksi | ASTM D882 |
Honeywell Halar® High Performance E-CTFE Film
(discontinued **) Description: Halar® is a high performance Ethylene-Chlorotrifluoroethylene (E-CTFE) film with excellent mechanical, electrical and release properties. It is non-flammable, and has outstanding chem.. |