Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Secant Modulus, TD | 0.00145 - 0.869 GPa | 0.210 - 126 ksi | Average value: 0.222 GPa Grade Count:194 |
Overview of materials for Linear Low Density Polyethylene (LLDPE), Film Grade This property data is a summary of similar materials in the MatWeb database for the category "Linear Low Density Polyethylene (LLDPE), Film Grade". Each property range of values reported is minimum .. |