Polymer Property : Secant Modulus, TD = 0.724 GPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Secant Modulus, TD 0.724 - 1.275 GPa
105 - 184.9 ksi
ASTM D882
Honeywell Capran® K Coated Nylon Film  (discontinued **)
Description: Capran® K is a PVdc coated nylon 6 film designed for food packaging applications where longer shelf life is required. This film exhibits good clarity, gloss, toughness, thermoformabil..
Secant Modulus, TD 0.724 - 1.275 GPa
105 - 184.9 ksi
ASTM D882
Honeywell Capran® Nylon Film, Multipurpose Nylon 6 Film
Description: Capran® is a multipurpose nylon 6 film. Its physical properties are evenly distributed for optimum performance giving excellent resistance to flex cracking. It can be processed ove..