Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Secant Modulus, TD | 0.520 GPa | 75.4 ksi | ASTM D882 |
NOVA Chemicals Sclair® 14G Butene LMDPE Film Resin Film Properties. Features: Low gel, good opacity, easy processability.Applications: Overwrap film.Data provided by the manufacturer. |
|||
Secant Modulus, TD | 0.520 GPa | 75.4 ksi | ASTM D882 |
Huntsman Rexell® M3109 Blown Film Extrusion LLDPE
(discontinued **) Linear-low medium density copolymer and FDA compliant.Features: Excellent combination of stiffness, heat resistance, and impermeability to water vapor.Applications: Food packaging, multi-layer syste.. |