Polymer Property : Secant Modulus, TD = 0.480 GPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Secant Modulus, TD 0.480 GPa
69.6 ksi
ASTM D882
Chevron Phillips HiD® 9638 HDPE Sheeting and Blown Film Resin  (discontinued **)
Resin Type: Sheeting Resin for the Geomembrane Market; ASTM D 4976 Classification: PE 225, A 56507Applications:Cast Geomembrane Applications, Notion and Millinery Bags, Heavy Duty Shipping Sacks, In..