Mechanical Properties Metric English Comments
Secant Modulus, TD 0.337 GPa
48.9 ksi
ASTM D882
Chevron Phillips 7109BK Linear low density polyethylene blown film resin  (discontinued **)
Resin Type: linear low density polyethylene, hexene copolymer, blow film resin, medium slip, medium antiblock version of 7109Characteristics: good stiffness at thin gauges, good drawdown, low COF, c..