Polymer Property : Secant Modulus, TD = 0.276 GPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Secant Modulus, TD 0.152 - 0.276 GPa
22.0 - 40.0 ksi
Average value: 0.218 GPa Grade Count:12
Overview of materials for Low Density Polyethylene (LDPE), Molded
This property data is a summary of similar materials in the MatWeb database for the category "Low Density Polyethylene (LDPE), Molded". Each property range of values reported is minimum and maximum ..