Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Secant Modulus, TD | 0.242 GPa | 35.1 ksi | ASTM D882 |
Huntsman PE1031 Film Extrusion Polyethylene
(discontinued **) Homopolymer, and FDA compliant.Features: Superior strength, good machinability, and heat seal characteristics.Applications: Film extrusion: clarity packaging, frozen food, produce bags, shrink, bund.. |
|||
Secant Modulus, TD | 0.242 GPa | 35.1 ksi | ASTM D882 |
Huntsman PE1037 Film Extrusion Polyethylene
(discontinued **) Homopolymer, and FDA compliant.Features: Medium clarity packaging film and good draw down characteristics.Applications: Film extrusion: general purpose packaging and film applications.FDA Notes: Con.. |
|||
Secant Modulus, TD | 0.242 GPa | 35.1 ksi | ASTM D882 |
Huntsman PE1044 Film Extrusion Polyethylene
(discontinued **) Homopolymer, and FDA compliant.Features: Yields film with excellent optical and machinability.Applications: Film extrusion: soft goods and other high clarity packaging.FDA Notes: Conforms to FDA reg.. |
|||
Secant Modulus, TD | 0.242 GPa | 35.1 ksi | ASTM D882 |
Huntsman PE1055 Film Extrusion Polyethylene
(discontinued **) Homopolymer, and FDA compliant.Features: Yields film with excellent optical and draw down characteristicsApplications: Film extrusion: soft goods and other high clarity packaging.FDA Notes: Conforms.. |
|||
Secant Modulus, TD | 0.242 GPa | 35.1 ksi | ASTM D882 |
Huntsman PE1061 Film Extrusion Polyethylene
(discontinued **) Homopolymer and FDA compliant.Features: Exceptional strength, good machinability and heat seal characteristics.Applications: Film extrusion: high clarity packaging, frozen food, produce bags, shrink.. |