Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Secant Modulus, TD | 0.205 GPa | 29.7 ksi | 1%; ASTM D882 |
Braskem LF 0720/20 AF LLDPE Blown Film Extrusion Polyethylene 38µm film gauge, obtained in 40mm extruder, with blow up ratio 2, 2:1Applications: Heavy duty bags; "liners"; general purpose; HDPE and LDPE blends. Information provided by Braskem |